Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.80 GPa @Temperature 150 °C |
406 ksi @Temperature 302 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Tensile Modulus | 2.80 GPa @Temperature 60.0 °C |
406 ksi @Temperature 140 °F |
|
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
|
LATI Lapex R PPSU Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 90.0 °C |
406 ksi @Temperature 194 °F |
|
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
|
LATI Latamid 6 BH PA 6, Heat Stabilized Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 150 °C |
406 ksi @Temperature 302 °F |
|
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 150 °C |
406 ksi @Temperature 302 °F |
|
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 90.0 °C |
406 ksi @Temperature 194 °F |
|
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 150 °C |
406 ksi @Temperature 302 °F |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |
|||
Tensile Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
|
LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 150 °C |
406 ksi @Temperature 302 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Tensile Modulus | 2.80 GPa @Temperature 90.0 °C |
406 ksi @Temperature 194 °F |
|
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |