Mechanical Properties Metric English Comments
Tensile Modulus 3.60 GPa

@Temperature 23.0 °C
522 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 3.60 GPa

@Temperature 90.0 °C
522 ksi

@Temperature 194 °F
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm..
Tensile Modulus 3.60 GPa

@Temperature 120 °C
522 ksi

@Temperature 248 °F
LATI Larpeek 10 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Modulus 3.60 GPa

@Temperature 90.0 °C
522 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Modulus 3.60 GPa

@Temperature 150 °C
522 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin..
Tensile Modulus 3.60 GPa

@Temperature 120 °C
522 ksi

@Temperature 248 °F
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Tensile Modulus 3.60 GPa

@Temperature 120 °C
522 ksi

@Temperature 248 °F
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Modulus 3.60 GPa

@Temperature 60.0 °C
522 ksi

@Temperature 140 °F
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Modulus 3.60 GPa

@Temperature 60.0 °C
522 ksi

@Temperature 140 °F
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced
ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 3.60 GPa

@Temperature 120 °C
522 ksi

@Temperature 248 °F
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Tensile Modulus 3.60 GPa

@Temperature 150 °C
522 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Modulus 3.60 GPa

@Temperature 90.0 °C
522 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe..
Tensile Modulus 3.60 GPa

@Temperature 150 °C
522 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 3.60 GPa

@Temperature 23.0 °C
522 ksi

@Temperature 73.4 °F
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..