Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Nylene® Norpex® AX235 PPE (Polyphenylene Ether) Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® GX3800F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® INP581 ABS High flow, low molecular weight SAN.
Can be used as compounding additives for polymer blends.
Can be blended with high rubber graft modifier resins to produce customized ABS properties.
Suitable for.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 - 128 MPa | 9570 - 18600 psi | Average value: 108 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet
(discontinued **) Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Ineos Nova 1510 High Heat Crystal Polystyrene High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP SG004 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SG004 is a compound based on PA 12 resin containing Graphite. Added features include: Internally Lubricated. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AE003 ABS (Europe-Africa-Middle East) LNP* STATKON* AE003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features inclurde : Electrically Conductive. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 364 PBT+PC Designed for outdoor telecommunications enclosure applications. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan EX401 Copolyester Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, .. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |