Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistance, fire retardancy, excellent fabrication qualities, resistance to cracking and chipping, very low moisture absorption, thermoformability, flexibility, flexibility to allow small radius bendsFabrication: Kydex L can be thermoformed to produce 3 dimensional pars with excellent detail. It is easy to work and can be drilled, punched, brake formed, or routed using standard metal and/or woodworking equipment. Kydex L is not recommended for use on horizontal surfaces where hot items may be placed such as kitchen countertops and is not recommended for field application to walls as a wallcovering material.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 110 %
110 %
Modulus of Elasticity 2.482 GPa
360.0 ksi
Flexural Yield Strength 66.0 MPa
9570 psi
ASTM D790
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.5 °C
168 °F
annealed; ASTM D648
UL RTI, Electrical 50.0 °C

@Thickness 0.700 - 3.00 mm
122 °F

@Thickness 0.0276 - 0.118 in
UL RTI, Mechanical with Impact 50.0 °C

@Thickness 0.700 - 3.00 mm
122 °F

@Thickness 0.0276 - 0.118 in
UL RTI, Mechanical without Impact 50.0 °C

@Thickness 0.700 - 3.00 mm
122 °F

@Thickness 0.0276 - 0.118 in
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature