Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 85.5 MPa @Thickness 3.17 mm |
12400 psi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 85.5 MPa | 12400 psi | ASTM D790 |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 85.5 MPa | 12400 psi | ASTM D790 |
PTS POM-90 9.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 85.3 MPa @Thickness 3.20 mm |
12400 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON TR1000 PMMA+CNT Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG .. |
|||
Flexural Yield Strength | 85.5 MPa @Thickness 3.17 mm |
12400 psi @Thickness 0.125 in |
|
KEP Kepital® F20-52 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 85.3 MPa @Thickness 3.20 mm |
12400 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 85.3 MPa @Thickness 3.20 mm |
12400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 85.5 MPa | 12400 psi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 5230 Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 85.3 MPa @Thickness 3.20 mm |
12400 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY NS5000C PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |