Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | 15 mm/min. ASTM D790 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Flexural Yield Strength | 72.4 - 138 MPa | 10500 - 20000 psi | Average value: 103 MPa Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 72.4 - 303 MPa | 10500 - 44000 psi | Average value: 193 MPa Grade Count:120 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 3.20 mm |
10500 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM-D790 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 3.20 mm |
10500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 6.40 mm |
10500 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | ASTM D790 |
IRPC Polimaxx Polene 2511HX GA5 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 25% GLASS FIBRE REINFORCED VERY HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, LOW SHRINKAGE, HIGH STIFFNESS, CONTAIN UV STABILIZER AND LONG TERM.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Techmer ES Plastiblend® PA6 SF76 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (76%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Techmer ES Plastiblend® PA6 SF80 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (80%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | 15 mm/min. ASTM D790 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | ASTM D790 |
Samyang Trimma® SD6350H PMMA, Opaque High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded Compression molded Absylux ABS is a low cost engineering plastic ideal for prototyping. It has excellent dimensional stability and lends itself to all forms of fabricationInformation provided by We.. |
|||
Flexural Yield Strength | 72.4 MPa @Thickness 6.35 mm |
10500 psi @Thickness 0.250 in |
2.8 mm/min; ASTM D790 |
Chi Mei Kibilac® PW-978B ASA, High Heat Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation |
|||
Flexural Yield Strength | 72.4 - 179 MPa | 10500 - 26000 psi | Average value: 120 MPa Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
PlastxWorld CEVIAN®-V 400N ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 72.4 MPa | 10500 psi | ASTM D790 |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 3.20 mm |
10500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.4 MPa @Thickness 6.35 mm |
10500 psi @Thickness 0.250 in |
2.8 mm/min; ASTM D790 |
Chi Mei Kibilac® PW-978D ASA, High Heat
(discontinued **) Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation |