Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS PC/ABS with high stiffness and impact performance |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EX9332T PC (Europe-Africa-Middle East) LEXAN* EX9332T polycarbonate resin, MVR (300C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retadant, mold release, UV stabilized, transparent, translucent and opaque colors. Materi.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS7R PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East) LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific) Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Flexural Yield Strength | 95.0 - 234 MPa | 13800 - 34000 psi | Average value: 148 MPa Grade Count:31 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL REN501 PPE+PS Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX89795 PC (Europe-Africa-Middle East) LNP* STATKON* DX89795 is a compound based on Polycarbone resin containing Carbon Powder. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
Eurostar Starflam PX07037 PA6, Flame Retardant, Injection Molded Starflam PX07037 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (IR laser marking grade)Information provided by Eurostar. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content. |