Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by.. |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 3.20 mm |
9960 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 3.20 mm |
9960 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP2100 PP+GF10% Description: Injection Molding, PP+GF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 3.20 mm |
9960 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 3.20 mm |
9960 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 68.6 MPa | 9960 psi | ASTM D790 |
GRECO ISOPAK 540 ABS Resin Flame Retardant GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Yield Strength | 68.6 MPa | 9960 psi | ASTM D790 |
GRECO ISOPAK 569 ABS Resin Extrusion GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical TR300 MABS, Flame Retardant, Transparency Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch.. |
|||
Flexural Yield Strength | 68.6 MPa | 9950 psi | ASTM D790 |
Hannam Chemical Hanalac H-2938 ABS |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5011 PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 68.6 MPa | 9960 psi | ASTM D790 |
Cheng Yu Plastic ML848 Flame Retardant PC |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-14S ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa | 9960 psi | ASTM D790 |
Cheng Yu Plastic ML1010 PC/PTFE |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade Information provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-14S ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade Information provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |