Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 113 MPa | 16400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Europe-Africa-Middle East) CYCOLOY MC5220 is a 20% glass reinforced PC+ABS blend for injection moulding purposes. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Flexural Yield Strength | 113 - 200 MPa | 16400 - 29000 psi | Average value: 160 MPa Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Flexural Yield Strength | 113 MPa @Thickness 6.40 mm |
16400 psi @Thickness 0.252 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 113 MPa @Thickness 3.20 mm |
16400 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 113 MPa @Thickness 3.20 mm |
16400 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 113 MPa @Thickness 3.20 mm |
16400 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 50 mm/min; ASTM D790 |
LG Chemical 81HF SAN Resin High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li.. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GX061104 PSU (Europe-Africa-Middle East) LNP* COLORCOMP* GX061104 is a compound based on Polysulfone resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | ASTM D790 |
Samyang Tramid® 210P Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl 534 PPE+PS High heat, unreinforced.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | ASTM D790 |
PlastxWorld CEVIAN® SERG3 30% GF ABS Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | ASTM D790 |
Cheng Yu Plastic N6CV1 Flame Retardant Nylon 6, 10% Mineral Reinforced |
|||
Flexural Yield Strength | 113 MPa | 16400 psi | 2 mm/min; ISO 178 |
Eurostar Starglas GX061104 PSU Starglas GX061104 is a PSU resin (also known as Starglas PSU A ¾)Information provided by Eurostar. |
|||
Flexural Yield Strength | 113 MPa @Thickness 6.40 mm |
16400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Flexural Yield Strength | 113 MPa @Thickness 6.40 mm |
16400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |