Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil LL 1237x98 Cast Film Resin
(discontinued **) LL 1237x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Eastman E6838-997F Polyethylene
(discontinued **) E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1205 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 1184 |
Carmel Olefins IPETHENE® 214 Low Density Polyethylene
(discontinued **) IPETHENE® 214 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. APPLICATIONS IPETHENE® 214 is main.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D-882 |
Bapolene® 200B Polyethylene, Film Extrusion Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D-882 |
Bapolene® 222B Polyethylene Film Grade Bapolene 222B is a butene linear low density polyethylene for blown film applications requiring superior impact strength and toughness. It complies with US FDA 21CFR177.1520.Applications: General p.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 1184 |
Carmel Olefins IPETHENE® 213 Low Density Polyethylene IPETHENE® 213 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between .. |
|||
Film Tensile Strength at Break, TD | >= 19.0 MPa | >= 2760 psi | ASTM D882 |
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A.. |
|||
Film Tensile Strength at Break, TD | >= 19.0 MPa | >= 2760 psi | ASTM D882 |
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1078 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | |
Reliance Industries LLDPE film - Active alumina + zeolite based film Information provided by Reliance Industries |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1203 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1345 EVA Film Extrusion
(discontinued **) 3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE 1375 EVA Film Extrusion