Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 200 g | 0.441 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:.. |
|||
Dart Drop Test | >= 200 g | >= 0.441 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 200 g | 0.441 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
SABIC HP0322N Low Density Polyethylene for Blown Film Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
Dart Drop Test | 200 g | 0.441 lb | |
DuPont™ Sclairfilm® MPP-1 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Dart Drop Test | 200 g | 0.441 lb | |
DuPont™ Sclairfilm® MPP-3 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Dart Drop Test | 200 g | 0.441 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Dart Drop Test | 200 g | 0.441 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
Huntsman PE1503 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
Huntsman PE1504 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
Huntsman PE1605 EVA Film Extrusion
(discontinued **) 6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Dart Drop Test | 200 g | 0.441 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
Formosa Plastics Formolene® E925 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E925 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709A |
ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709A |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM-D1709 |
Braskem LL5800N LLDPE Blown Film Extrusion Polyethylene Copolymer LL5800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM-D1709 |
Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer The LL5801N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing .. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM-D1709 |
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ASTM D1709 |
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A.. |
|||
Dart Drop Test | 200 g | 0.441 lb | ISO 7765-1 |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion .. |
|||
Dart Drop Test | 200 g | 0.441 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |