Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer Total Atofina
Trade Name Lumicene® mPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion pressure, excellent bubble stability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The combination of these features brings a significant downgauging potential.Lumicene® mPE M 2710 EP is especially dedicated to film applications where high gloss and high transparency are required, particularly in blend and coextrusion with LLDPE or LDPE.Lumicene® mPE M 2710 EP is suited for many applications in the field of consumer, industrial, food or hygiene packaging such as bags, deep freeze, collation shrink and lamination.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.927 g/cc
0.927 g/cc
ISO 1183
Thickness 40.0 microns
1.57 mil
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.5 MPa
1960 psi
ISO 527-3
Film Tensile Strength at Yield, TD 14.0 MPa
2030 psi
ISO 527-3
Film Elongation at Break, MD 650 %
650 %
ISO 527-3
Film Elongation at Break, TD 720 %
720 %
ISO 527-3
Elmendorf Tear Strength, MD 6.10 g/micron
155 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 16.3 g/micron
414 g/mil
ISO 6383-2
Dart Drop Test 200 g
0.441 lb
ISO 7765-1
Film Tensile Strength at Break, MD 51.0 MPa
7400 psi
ISO 527-3
Film Tensile Strength at Break, TD 48.0 MPa
6960 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 119 °C
246 °F
ISO 11357
Vicat Softening Point 118 °C
244 °F
ISO 306
Optical Properties Metric English Comments
Haze 6.5 %
6.5 %
ISO 14782
Gloss 70 %
70 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 180 - 230 °C
356 - 446 °F
Blow Molding
Melt Temperature 200 °C
392 °F
Extrusion
Die Opening 0.0800 - 0.280 cm
0.0315 - 0.110 in
Blow-up Ratio (BUR) 1.5 - 4.5
1.5 - 4.5