Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 150 g | 0.331 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |
|||
Dart Drop Test | 150 g | 0.331 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |
|||
Dart Drop Test | >= 150 g | >= 0.331 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 150 g | 0.331 lb | 50µ; ISO 7765-1 |
Total Lacqtene® 1003 FE 30 HDPE, blow molding
(discontinued **) Medium density radical polyethylene made by high tubular pressure process for medical applications requiring sterilization : small and medium stiff containers for parental mixtures, ophthalmic solut.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop Test | 150 g | 0.331 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Dart Drop Test | 150 g | 0.331 lb | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 214 Low Density Polyethylene
(discontinued **) IPETHENE® 214 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. APPLICATIONS IPETHENE® 214 is main.. |
|||
Dart Drop Test | 150 g | 0.331 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
Dart Drop Test | 150 g | 0.331 lb | Using 2 in. (0.508 cm) dia dart, 60 in. (774 cm) drop height. |
Kraton® D1102 + HDPE blend (15/85) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
SIDPEC EGYPTENE® HD 5301 FB HDPE Film Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation .. |
|||
Dart Drop Test | 150 g | 0.331 lb | ISO 7765-1 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ISO 7765-1 |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
Dart Drop Test | 150 g | 0.331 lb | F50; ASTM D1709 |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Dart Drop Test | 150 g | 0.331 lb | F50; ASTM D1709 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709, A |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
Dart Drop Test | 150 g | 0.331 lb | 1.0 mil; ASTM D 1709 |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM-D1709 |
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional .. |
|||
Dart Drop Test | 150 g | 0.331 lb | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 210 Low Density Polyethylene IPETHENE® 210 is a low density polyethylene extrusion grade, containing no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 210 is mainly u.. |
|||
Dart Drop Test | 150 g | 0.331 lb | 50µ; ISO 7765-1 |
Total Lacqtene® 1008 FE 30 LDPE blown film
(discontinued **) Low density radical polyethylene made by high pressure autoclave process. Grade for very stiff and transparent thin film. Applications examples: rigid bags, automatic packaging, thin shrink film.. A.. |
|||
Dart Drop Test | 150 g | 0.331 lb | F50; ISO 7765-1 |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
ExxonMobil Exceed™ 2227ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2227ED is a metallocene ethylene-hexene copolymer. It offers an excellent balance of high modulus and impact strength. The higher melt index makes it ideally suited for L.. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
Huntsman PE1335 EVA Film Extrusion
(discontinued **) 3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop Test | 150 g | 0.331 lb | ASTM D1709 |
Huntsman PE1345 EVA Film Extrusion
(discontinued **) 3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |