Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
SABIC 120W Linear Low Density Polyethylene for Blown Film Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, bags-on-roll, garment film.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D 882 |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LGH 138 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 138 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, slip agent, antiblocking and processing aid, suitable for blown film extrusion.Films obtai.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
ExxonMobil Escorene® LD-144 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, general purpose packaging, garment film.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0318-E Butene LLDPE Film Resin PF-0318-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ISO 527-3 |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Yield, TD | 9.00 - 11.0 MPa | 1310 - 1600 psi | Average value: 9.81 MPa Grade Count:7 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
(discontinued **) Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced.. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin
(discontinued **) Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but .. |
|||
Film Tensile Strength at Yield, TD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |