Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.00 GPa | 725 ksi | ASTM D638M-93 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)
(discontinued **)&l The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ASTM D638 |
Loxim 220 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PB00A PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PB00A is a compound based on PA 6 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 5.00 GPa @Temperature 160 °C |
725 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-23 ESD PA12-GF23 Product description: Grilamid LV-23 ESD is a 20% fiber reinforced, anti-static injection molding grade Polyamide 12 (PA12). Grilamid LV-23 ESD is heat stabilized, is easy to process and demold. The .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 22C BK086 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C BK086 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
DSM Akulon® S223-GM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-2 |
CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resista.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1mm/min; ISO 527 |
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | Longitudinal |
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-2 |
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p.. |