Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.75 GPa | 399 ksi | |
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electrical purposes. Excellent flow of the material predetermines it for.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527-1/-2 |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific) LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ASTM D638 |
Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527 |
Eurotec® Tecodur® PB70 NL RT PBT, unfilled, PTFE modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527 |
Eurotec® Tecodur® PB70 NL XA 20 PBT unreinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527 |
Eurotec® Tecomid® NT40 NL MB PPA, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Plastcom SLOVALEN PH 73 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Henkel Hysol EA 9396 Paste Adhesive System Two-part, low viscosity, unfilled version of Hysol EA 9394. Qualified to BMS 8-301.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |