Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.45 GPa | 355 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | Type I; ASTM D638 |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data) Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EX2079X PC (Europe-Africa-Middle East) Lexan* EX2079X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/2 |
PTS POM-90 Acetal Copolymer Information provided by PTS LLC. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002PC PC LNP* LUBRICOMP* DL002PC is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this grade are: Wear Resistant, Exceptional Processing, Clean Compound System. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EX2078X PC (Europe-Africa-Middle East) Lexan* EX2078X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1040 PP SABIC® PPcompound 55T1040 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact and high rigidity, and is suitable for injec.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific) LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1mm/min; ISO 527 |
Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy General grade of PC/ABS polymer alloy, having improved impact strength and heat resistance compared with a heat resistant ABS and flame retardant m-PPE and also having higher fluidity compared with .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific) LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Apec® FR1892 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
Covestro Bayblend® W85 XF* Polycarbonate + ASA Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Dow SiLK™ I 130 Semiconductor Dielectric Resin SiLK™ I 130 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 130 is compatible with.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Dow SiLK™ I 360 Semiconductor Dielectric Resin SiLK™ I 360 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 360 is compatible with.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Dow SiLK™ I300 140 Semiconductor Dielectric Resin SiLK™ I300 140 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 140 is compatibl.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |