Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.42 GPa | 351 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | TD; ASTM D638 |
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ1022 PC Standard Flow OQ Resin |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific) Standard Flow OQ Resin |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ1022 PC (Europe-Africa-Middle East) Standard Flow OQ Resin |
|||
Tensile Modulus | 2.42 GPa @Temperature 23.0 °C |
351 ksi @Temperature 73.4 °F |
1-mm/min; ISO 527 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | ISO 527-1/-2 |
Kuraray Genestarâ„¢ N1001A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific) LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON FX91304 PE LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Valox® SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled productThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled product |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ CMU 236 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness/toughness balance is required.Availa.. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Tensile Modulus | 2.42 GPa | 351 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |