Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific) Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1mm/min |
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.09 GPa @Thickness 3.20 mm |
303 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific) LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA 11 (Asia Pacific) LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing Glass Bead. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11 LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1mm/min |
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 2.09 GPa @Temperature 120 °C |
303 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min |
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic.. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Modulus | 2.09 GPa | 303 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated. |