Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.00 GPa | 290 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PH 52 T 20 003/1M Polypropylene reinforced with 20% mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 6 BT PA6 Basic type PA 6 for compounding, modified for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Informa.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex KS003AI Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS003AI is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include; EMI/RFI Shielding, Electrically Conductive.This data was supplied by SAB.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FL900P PC (Europe-Africa-Middle East) Foamable LEXAN, various weight reductions at 6.4 mm. Offers load bearing capability at elavated temp., Combines rigidity, impact & toughness.This data was supplied by SABIC-IP for the Europe-Africa-.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 221 PA66, Conditioned Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Spartech SP-9030 Economy ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East) Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Star Plastics ABS5035 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
Styrolution PS 641F HIPS Styrolution PS 641F is high impact polystyrene with high heat resistance.High impactHigh heat resistanceInformation provided by Styrolution |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
Wanshijie PC Film PC is a kind of shapeless, odorless, non-toxic, high transparency, colorless or light yellow thermoplastic engineering plastic with excellent physical and mechanical properties, especially excellent.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
Polyram RamTough PZ506 Polycarbonate, UV Stabilized, Flame Retardant UV stabilized, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-2 |
Total PPH 9040 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9040 is a nucleated homopolymer. PPH 9040 is characterized by an improved rigidity and high clarity .ApplicationATOFINA Polypropylene PPH 9040 is suitable for the injectio.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Americas Styrenics STYRON® 487R High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer.. |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
Aclo Accucomp ABS ABS801V Automotive Approved Grade |
|||
Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |