Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.86 GPa | 270 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Spartech SP-2010 HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM Data |
Styron Magnumâ„¢ FG960 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM Data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Lubrizol Hipscon™ B-515 Static Control Polystyrene Hipscon™ B-515 is a carbon black-filled, Polystyrene compound available in compound form. Hipscom™ B-515 compound maintains extremely low gloss surfaces after molding, allowing for easy reading o.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Total PSI 945 Polystyrene Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Lubrizol Hipscon™ M-520 Static Control High Impact Polystyrene Hipscon™ M-520 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are easily formed into deep pockets that maintain uniform static protec.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | TM R050-36 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ASTM D638 |
American Polymers API 645-21 Polystyrene API 645-21 is a super high impact polystyrene used in applications requiring a superior level of toughness along with good tensile and flexural properties. On balance this extrusion grade polymer a.. |
|||
Tensile Modulus | 1.86 GPa | 270 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |