Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.38 GPa | 200 ksi | |
Plastcom SLOVALEN PQ 83 T 15 PP, 15% mineral filling, UV stabilization FeaturesModified PP for injection moulding with the content of 15% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet) Natural and Black |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM Data |
Americas Styrenics Styron® 6187SF High Impact Polystyrene
(discontinued **) STYRON® 6187SF structural foam molding resin is a high impact polystyrene grade with proprietary ignition resistance additive package to achieve UL 94 V-0 rating. It offers excellent moldability an.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | |
Ineos Styrenics Polystyrene 476M Q598 (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM Test |
Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM Test |
Styrolution Terblend® N NM-19 ABS/PA6 (Conditioned) Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM Test |
Styrolution Terblend® N NMX04 ABS/PA6 (Conditioned) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Lubrizol Hipscon™ M-530 Static Control Polystyrene Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unif.. |
|||
Tensile Modulus | 1.38 - 1.72 GPa @Temperature 23.9 °C |
200 - 250 ksi @Temperature 75.0 °F |
|
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Tensile Modulus | >= 1.38 GPa | >= 200 ksi | |
Master Bond LED401 White One Part, LED Curable Compound Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | TM R050-36 |
Resinlab® EP1300 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Clear (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |