| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
| Water Absorption | <= 0.040 % | <= 0.040 % | ASTM D257 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 78 | 78 | ASTM D2240 |
| Tensile Strength | 34.5 MPa | 5000 psi | ASTM D638, ASTM D1708 |
| Elongation at Break | 150 % | 150 % | ASTM D638, ASTM D1708 |
| Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
| Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
| Compressive Strength | 80.0 MPa | 11600 psi | ASTM D695 |
| Izod Impact, Notched | 1.60 - 3.20 J/cm | 3.00 - 6.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.187 W/m-K | 1.30 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 160 °C | 320 °F | |
| Maximum Service Temperature, Air | 150 °C | 302 °F | Continuous |
| Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 44 % | 44 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 7.2 @Frequency 1000 Hz |
7.2 @Frequency 1000 Hz |
ASTM D150 |
| 8.5 @Frequency 1.00e+6 Hz |
8.5 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 63.0 kV/mm | 1600 kV/in | Short Term; 10 mil film; ASTM D149 |
| Dissipation Factor | 0.030 @Frequency 1000 Hz |
0.030 @Frequency 1000 Hz |
ASTM D150 |
| 0.090 @Frequency 1.00e+6 Hz |
0.090 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chemical Resistance | Good | |
| Weather Resistance | Excellent |