Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Semitron® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Water Absorption | 2.0 % | 2.0 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | 8.0 % | 8.0 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 50 | 50 | ASTM D785 |
Hardness, Rockwell R | 108 | 108 | ASTM D785 |
Hardness, Shore D | 76 | 76 | ASTM D2240 |
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D638 |
Elongation at Break | 15 % | 15 % | ASTM D638 |
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Compressive Strength | 55.2 MPa | 8000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 1.21 GPa | 175 ksi | ASTM D695 |
Shear Strength | 41.4 MPa | 6000 psi | ASTM D732 |
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 Type A |
Coefficient of Friction, Dynamic | 0.29 | 0.29 | Dry vs. Steel; QTM55007 |
K (wear) Factor | 60.4 x 10-8 mm³/N-M | 30.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 167 µm/m-°C @Temperature -40.0 - 149 °C |
93.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Melting Point | 160 °C | 320 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | EOS/ESD S11.11 |
Dielectric Constant | 4.31 @Frequency 1e+6 Hz |
4.31 @Frequency 1e+6 Hz |
ASTM D150 |
Dissipation Factor | 0.036 @Frequency 1e+6 Hz |
0.036 @Frequency 1e+6 Hz |
ASTM D150 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
Acids, Weak | Limited | Limited | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
Alkalies, Weak | Acceptable | Acceptable | |
Chlorinated Solvents | Limited | Limited | |
Conductive / Static Dissipative | Yes | Yes | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Acceptable | Acceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Machinability | 1 | 1-10, 1=Easier to Machine |