Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.4 GPa | 1650 ksi | |
Radici Radiflam® S RV300AE (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | LW; ASTM D638 |
Haysite H1000 Polyester Laminate Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | |
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | |
LATI Latimass 62-07 D025 PA6, Impact Modified Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ASTM D638 |
Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 LNP THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% Milled Glass. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABI.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6 LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1015G35 NAT PA6-GF35 35% Glass Reinforced, Injection Molding |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL BK039B is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |