Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | |
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1 |
Iran Petrochemical (PCC) HB5020 High Density Polyethylene HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1mm/min; ISO 527-2 |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1mm/min; ISO 527-2 |
Borealis Borclear™ RC707MO Polypropylene Borclear™ RC707MO is intended for blow molding. This grade provides high gloss, high transparency and excellent impact properties. This grade also features high heat distortion temperature. Applic.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | At 1 mm/min; ASTM D638 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | MD; ASTM D882-A |
Borealis FS1560 High Density Polyethylene FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 572-2 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
DSM Akulon® F223-D (Cond.) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
DSM Akulon® K125/A PA6 Low Viscosity |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
DSM Stanyl® TW300 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | Through Plane Direction |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Aclo Accucomp Polypropylene CPO406L Copolymer |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T10L1 Talc Reinforced |
|||
Tensile Modulus | 1.00 GPa | 145 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |