Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | |
Radici Radilon® S RCV3515 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | |
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Tensile Modulus | 5.00 GPa @Thickness 0.0250 mm |
725 ksi @Thickness 0.000984 in |
MD; ISO 527 |
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-3830 30% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-3830 is a 30% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3830 is recommended for producing in.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Polyram RamLloy PN300G4 PPE/PS Alloy, 20% Glass Fiber PPE/PS alloy, 20% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Polyram RamTough PZ307G4 Polycarbonate, 20% Glass Fiber, UV Stabilized 20% glass fiber reinforced polycarbonate, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Polyram Polytron P20B03 Polypropylene, 20% Long Glass Fiber A chemically coupled 20% long glass fibers reinforced black polypropylene, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 5.00 - 5.50 GPa | 725 - 798 ksi | biax film |
Goodfellow Polyethylene Naphthalate (PEN) Film A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colo.. |
|||
Tensile Modulus | 5.00 GPa @Temperature 160 °C |
725 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Eurotec® Tecomid® NB40 MR30 NL PA 6 30% mineral reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ASTM D638 |
Aclo Accutech Polypropylene CP0435G43CV Copolymer Glass Reinforced Coupled Approved to GMP.PP.039 Black A13054 |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Conditioned, 23% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | |
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |