Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.75 GPa | 399 ksi | |
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527-1/2 |
Radici Raditer® BN100 Polybutylene Terephthalate PBT General PurposeInformation provided by Radici group. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | Molded; ASTM D882 |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ASTM D638 |
Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ HMU 208 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and release agent for automotive HVAC and under-the-hood applications.Availability: Africa & Middl.. |
|||
Tensile Modulus | 2.75 GPa | 400 ksi | Storage |
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding... |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527 |
Eurotec® Tecotek® PC40 NL FA70 PC, unfilled, flame retardant - (RoHS compliant), natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527-1/-2 |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Plastcom SLOVALEN PH 73 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Henkel Hysol EA 9396 Paste Adhesive System Two-part, low viscosity, unfilled version of Hysol EA 9394. Qualified to BMS 8-301.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Henkel SynCore 9872.1 Syntactic Film Toughened, low density syntactic core, superior moisture resistance, co-curable with a wide variety of 350°F / 177°C curing epoxy prepregs. |