Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel SynCore 9872.1 Syntactic Film

Category Polymer , Film
Manufacturer Henkel
Trade Name SynCore
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel SynCore 9872.1 Syntactic Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Toughened, low density syntactic core, superior moisture resistance, co-curable with a wide variety of 350°F / 177°C curing epoxy prepregs.
Physical Properties Metric English Comments
Density 0.670 g/cc
0.0242 lb/in³
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 31.0 MPa
4500 psi
Tensile Modulus 2.75 GPa
399 ksi
Compressive Strength 61.0 MPa
8850 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Out-Time (days) 10
at 32°C
15
at 25°C
Users viewing this material also viewed the following: