Mechanical Properties Metric English Comments
Tensile Modulus 2.42 GPa
351 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Modulus 2.42 GPa
351 ksi
TD; ASTM D638
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East)
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market.
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 2.42 GPa
351 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® OQ1022 PC
Standard Flow OQ Resin
Tensile Modulus 2.42 GPa
351 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific)
Standard Flow OQ Resin
Tensile Modulus 2.42 GPa
351 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® OQ1022 PC (Europe-Africa-Middle East)
Standard Flow OQ Resin
Tensile Modulus 2.42 GPa

@Temperature 23.0 °C
351 ksi

@Temperature 73.4 °F
1-mm/min; ISO 527
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade
Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components.
Tensile Modulus 2.42 GPa
351 ksi
ISO 527-1/-2
Kuraray Genestarâ„¢ N1001A-M41 Nylon
Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel
Tensile Modulus 2.42 GPa
351 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated.
Tensile Modulus 2.42 GPa
351 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific)
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing.
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PVX516 PPE
PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific)
Low odor grade for IC tray application
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON FX91304 PE
LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Tensile Modulus 2.42 GPa
351 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Valox® SLWM2105 PBT+PC (Asia Pacific)
Anti-static PBT/PC blend, mineral 5% filled productThis data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 2.42 GPa
351 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific)
Anti-static PBT/PC blend, mineral 5% filled product
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East)
Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Tensile Modulus 2.42 GPa
351 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Tensile Modulus 2.42 GPa
351 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ CMU 236 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness/toughness balance is required.Availa..
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Tensile Modulus 2.42 GPa
351 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PX2060 PPE+PS
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..