Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Total 819E Polystyrene
(discontinued **) Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof.. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
LG Chemical Lupoy 1621-02 Polycarbonate Resin Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON CD0001 PS LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Star Plastics ABSHFL Molding Grade ABS High Flow Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific) LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Data |
Styron Magnum™ 9085 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Data |
Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Data |
Styron CALIBRE™ SF 7070 Polycarbonate, 7% Glass Reinforced Structural Foam Grade CALIBRE® SF7070. is a 7% glass reinforced structural foam ignition resistant polycarbonate resin specially developed for injection molding processing. The CALIBRE 7070 resin provides a high flexu.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ISO 527-2 |
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu.. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM 638 |
Chase Plastics CP Pryme® PC100RHF Polycarbonate Form: PelletsInformation provided by Chase Plastics. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |