Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® BY2710X PC (Asia Pacific) BY2710X is a modified Polycarbonate (PC) resin. It is a non-filled, injection moldable grade with UL-94 V0 rating and is available in various opaque color options. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | ASTM D638 |
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren.. |
|||
Tensile Modulus | 2.22 GPa @Thickness 3.20 mm |
321 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific) LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON FD000 PE LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | |
Stratasys® Ultem 9085 for Rapid Prototyping ULTEM* 9085 is a fl ame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high strength-to-weigh.. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Tensile Modulus | 2.22 GPa | 322 ksi | Storage |
Epoxy Technology EPO-TEK® 360 Low Viscosity Optical Epoxy Adhesive Product Description: EPO-TEK® 360 is a two component, high-temperature grade epoxy for semiconductor, electronics, fiber optics and medical applications.Advantages & Application Notes: Built in col.. |