Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.07 - 3.45 GPa | 300 - 500 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC) Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | X, Y-Direction; ASTM D638 |
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Fiberfil® J-61/10 Polypropylene Copolymer, 10% Glass Fiber Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type I, 51 mm/min; ASTM D638 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 780HP ABS, High Heat, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | >= 2.07 GPa | >= 300 ksi | |
Master Bond EP38CL Adhesive Features Toughness and Durability Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade TOTAL Petrochemicals 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination o.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D412 |
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | |
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | blown films TD; ISO 527-3 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ AT-000/000 ESD Acetal-Copolymer
(discontinued **) Description/Features:AntistaticInformation provided by PolyOne Corporation. |