Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.01 GPa | 292 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Geon™ L4605 Ivory 3098 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | ASTM D638 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 1mm/min |
Eastman Tenite 105-28 Cellulose Acetate
(discontinued **) 28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | ASTM D638 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | ASTM D638 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.01 GPa | 292 ksi | 1mm/min |
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 2.01 GPa @Temperature -50.0 °C |
292 ksi @Temperature -58.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |