Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.0 GPa | 2320 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-2 |
PolyOne OnForce™ LFT PP-60LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 16.0 GPa @Temperature 23.0 °C |
2320 ksi @Temperature 73.4 °F |
ISO 527 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 CF30 HWCP 30% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-1/-2 |
DSM Stanyl® TW241F10 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45 Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon .. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | 1 [mm/min]; ISO 527-2/1 |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Sorona® 2045G BK346A Polytrimethylene Terephthalate (PTT)
(Unverified Data**) 45% Glass Reinforced Polytrimethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |