Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ASTM D638 |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ASTM D638 |
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ASTM D638 |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Nilit FRIANYL B63 GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Nilit FRIANYL B63 H-GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | |
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10312 PA (Asia Pacific) 9X10312 is 50% glass fiber reinforced, impact modified nylon material. High modulus, high flow and good ductility, Low Moisture Absorption. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50 Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | |
Cytec Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527-1/-2 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Tensile Modulus | 15.0 GPa @Temperature 70.0 °C, Time 180000 sec |
2180 ksi @Temperature 158 °F, Time 50.0 hour |
62% RH |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
Tensile Modulus | 15.0 GPa | 2180 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated |