Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.4 GPa | 1650 ksi | |
Radici Radiflam® S RV300AE (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | |
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | |
LATI Latimass 62-07 D025 PA6, Impact Modified Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ASTM D638 |
Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific) LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 LNP THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% Milled Glass. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABI.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | ISO 527 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 (Asia Pacific) LNP* THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1015G35 NAT PA6-GF35 35% Glass Reinforced, Injection Molding |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL BK039B is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Modulus | 11.4 GPa | 1650 ksi | 1 mm/min |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |