Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-1/-2 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | |
Radici Radilon® A HS (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50 mm/min (2.0 in/min) |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer INNOPOL® CS 2-8000 is a polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8000 is highly suitable for pipe manufacturing where the required.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 402 Natural FA PA66, Conditioned Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 402H1 Natural PA66, Conditioned Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ASTM-D790 |
Polyram RamTal PM8515 Acetal, High impact High impact polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 20 nat PA610 Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HWCP Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 TLWCP Nylon 66, Flame Protection Grade V-2, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 139 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4188 nat PA612 Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosi.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | DIN 53 457 |
Hippe PP Polypropylene Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 6000 Nylon Alloy, Flexible Grade (Conditioned) LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 6000T Nylon Alloy, Flexible Grade (Conditioned) LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 12 Polyamide 12 This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50 mm/min (2.0 in/min) |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |