Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Orgalloy® LE 6000 Nylon Alloy, Flexible Grade (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon, Flexible Alloy
Manufacturer Arkema
Trade Name Orgalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orgalloy® LE 6000 Nylon Alloy, Flexible Grade (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of film, tube and hollow vessels. Also suited to injection moldingISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Water Absorption 6.4 %
6.4 %
Moisture Absorption at Equilibrium 1.8 %
1.8 %
Humidity Absorption
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 4.2 %
4.2 %
50 mm/min
Tensile Modulus 1.30 GPa
189 ksi
1 mm/min
Tensile Creep Modulus, 1 hour 1130 MPa
164000 psi
Tensile Creep Modulus, 1000 hours 520 MPa
75400 psi
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min
Vicat Softening Point 97.0 °C
207 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V