Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.15 GPa | 167 ksi | |
Radici Radilon® S 40E (cond.) Nylon 6 PA6 high viscosity injection molding suitable also for extrusion.Information provided by Radici group. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527 |
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9514 is a 10% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9514 is dev.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ HE9621-PH HDPE for Healthcare Applications Bormed HE9621-PH is a natural HD polyethylene with narrow molecular weight distribution, produced in low-pressure gas-phase process. This grade is designed for the injection molding of articles whe.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | At 1 mm/min; ASTM D638 |
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications Bormed RF825MO is a specially modified random copolymer polypropylene with high melt flow intended for use in medical and medical related articles. Bormed RF825MO is characterized by easy processab.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | At 1 mm/min; ASTM D638 |
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications Bormed RF830MO is a specialty modified random copolymer polypropylene with high melt flow intended for use in medical and medical related articles. Bormed RF830MO is characterized by easy processab.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ EE115AE TPO Compound Daplen EE115AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ EE115T TPO Compound Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-2 |
Borealis MG9621B Polyethylene Applications: crates, and pailsInformation provided by Borealis AG |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-2 |
Borealis MG9621S Polyethylene MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-2 |
Borealis RF926MO Polypropylene, Transparent Random Copolymer RF926MO is a specially modified transparent polypropylene random copolymer with high melt flow. This grade is intended for injection stretch blow molding (ISBM). and is designed for high-speed injec.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Total PPC 9712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-2 |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-3 |
Borealis RF365MO Polypropylene Applications: closures, thin wall containers, and excellent transparency.Information provided by Borealis AG |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ CNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications in which good surface finish and UV resistance is required. Availabilit.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO527-2/1 |
ExxonMobil PP7085E1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica.. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Domo 2448L Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Domo 2600M Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | ISO 527 |
Dow INSPIRE™ 112 Performance Polymer INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | |
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | |
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | |
BASF Novolen® 2660 M Polypropylene UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | |
BASF Procom® D 1118 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.15 GPa | 167 ksi | 1mm/min; ISO 527-2 |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |