ExxonMobil Exxtral™ CNU 011 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ CNU 011 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications in which good surface finish and UV resistance is required. Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessGood impact ResistanceGood Surface FinishLow EmissionsLow to No FoggingLow to No OdorUses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527-2/50
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2/50
Elongation at Break >= 100 %
>= 100 %
ISO 527-2/50
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50
Tensile Modulus 1.15 GPa
167 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.504 J/cm²

@Temperature 0.000 °C
2.40 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
0.840 J/cm²

@Temperature 22.8 °C
4.00 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C
163 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F
ISO 75-2/A