Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis MG9621B Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis MG9621B Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: crates, and pailsInformation provided by Borealis AG
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 868
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 200 - 260 °C
392 - 500 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Descriptive Properties Value Comments
Hold Pressure as low as possible
Injection Velocity as high as possible
Users viewing this material also viewed the following: