Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Novolen® 2600 M Polypropylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Novolen®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BASF Novolen® 2600 M Polypropylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection molded partsData was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Water Absorption 0.10 %
0.10 %
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 6.0 %
6.0 %
Tensile Modulus 1.15 GPa
167 ksi
Charpy Impact Unnotched NB
NB
17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 4.50 J/cm²
21.4 ft-lb/in²
0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
Melting Point 163 °C
325 °F
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Vicat Softening Point 58.0 °C
136 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
Dielectric Strength 140 kV/mm
3560 kV/in
Dissipation Factor 0.000070

@Frequency 100 Hz
0.000070

@Frequency 100 Hz
0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
600 V