Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East) LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ASTM-D638 |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ASTM-D638 |
Polyram RamTal PM1003 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ISO 527-1/-2 |
Covestro Bayblend® FR 3011 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegood flowhigh heat resistanceVicat/B 120 temperature = 118 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR XE 4010 PA*-I Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fat.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 |
Chi Mei Wonderlite® PC-108U Polycarbonate - UV Stabilized UV Stabilized |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ISO 527-1 |
Barlog Plastics KEBAFORM C 270.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ISO 527-1 |
Barlog Plastics KEBAFORM C 901 FA POM Copolymer unreinforced, reduced formaldehyde emission POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 2 in/min; ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ASTM D638 |
Ashley Polymers Ashlene® RH190H2-B Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized with carbon black for outstanding weatherability.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ISO 527-1/-2 |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Tensile Strength, Yield | 65.0 MPa | 9430 psi | ISO 527 |
Polyram RamTal PM1113 Polyacetal Copolymer for Injection Molding General purpose polyacetal copolymer for injection molding applications, MFI 13.Information provided by Polyram. |