Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific) Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific) AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY FXW750SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Med. Heat & Impact Resin |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 10%/min. ASTM D638 |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific) LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ASTM D 638 |
Cossa Polimeri ESTABLEND 6500 F Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh melt flow rate, good thermal resistance, good impact resistance, excellent processability, good surface appearanceInformation provided by .. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ASTM D 638 |
Cossa Polimeri ESTABLEND 6500 Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ASTM D638 |
E-Polymers Tekaloy® G70A3 , Heat Resistance, Easy Molding PC/ABS Alloy Heat Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ASTM D638 |
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy Non Halogen Flame Retardant, High FlowInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 340V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO value at 50 mm/min. |
BASF Capron® 8259 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8259 is a type 6 nylon injection molding graft copolymer developed for fastener applications requiring to abusive impact molding combined with a high level of pullout strength. It exhibits v.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Tensile Strength, Yield | 59.0 MPa | 8560 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |