Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS (Europe-Africa-Middle East) ABS plating grade optimized for a broad processing window for both painted and plated applications. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min |
Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1: PBT+PC (GF) Elastomer modified PBT+PC blend reinforced with 5% of glass fibres, a good combination of stiffness, dimensional stability and thoughness. Main applicat.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 150°C for 1,000 hrs; ASTM D1458 |
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | |
Ineos ABS Lustran® H606 LS Improved heat and UV resistance.,Property data per ISO test methods. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50mm/min; ISO 527 |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific) 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
Tensile Strength, Yield | 48.0 MPa @Strain 300 % |
6960 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8417 Polyurethane + ABS injection molding grademodified with ABSgood low-temperature flexibilitygood wear resistanceApplicationSki boot shellsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | parallel; ISO 527-3 |
Covestro Desmopan® W DP 89051D Polyurethane PreprocessingMax. Water content |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Diamond Polymers NYLON 6650HSL Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 2 in/min; ASTM Test |
BASF Ultramid® 8202C HS PA6 (Conditioned) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Ashley Polymers Ashlene® L930 Nylon 12 A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO 527 |
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry) Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Ashley Polymers Ashlene® 105 PBT Polyester A general purpose polyester with low shrinkage and good flow.Data provided by the manufacturer |