Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 47.6 MPa | 6900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ SF M7100 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ SF M7120 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
I. Stern WC-102 General Purpose Crystal Polystyrene Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. .. |
|||
Tensile Strength, Yield | 47.6 MPa @Thickness 3.20 mm |
6900 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ ABS-0500RX Biocompatible ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ ABS-0501A Antimicrobial ABS A high gloss, injection molding grade of ABS containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ ABS-0502AF Food Grade ABS A high gloss, injection molding grade of ABS with FDA food contact approval, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ ABS-0502ARX Biocompatible, Antimicrobial ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES Luriblend® PBT GB30 TL15 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM Data |
Styron Magnum™ 758HP ABS, High Heat, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES Electrablend® ABS SS16 FR BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES HiFill® PA6 0180 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM Data |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Techmer ES Plastiblend® ABS LE WT Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | 50 mm/min; ASTM D638 |
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | |
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D-638 |
Axiall 9275J Amber 05 Rigid PVC, Molding, Amber 05 Georgia Gulf 9275J Amber 05 is used for injection blow molded packages in cosmetic and toiletry applications. It is a pre-colored amber compound and all ingredients are FDA approved.Information pro.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D-638 |
Axiall 9275J Clear 40 Rigid PVC, Molding, Clear 40 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | ASTM D638 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Tensile Strength, Yield | 47.6 MPa | 6900 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ AT-000/000 ESD Acetal-Copolymer
(discontinued **) Description/Features:AntistaticInformation provided by PolyOne Corporation. |