Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® ABS LE WT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 47.6 MPa
6900 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 74.5 MPa
10800 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.900 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
1.01 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.90 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
2.19 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.4 °C
202 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648