Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Styron
Trade Name PULSE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Melt Flow 2.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 47.6 MPa
6900 psi
50 mm/min; ASTM D638
Flexural Modulus 2.18 GPa
316 ksi
ASTM D790
Izod Impact, Notched 5.10 J/cm

@Temperature -34.0 °C
9.55 ft-lb/in

@Temperature -29.2 °F
ASTM D256
6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
4.90 J/cm²

@Temperature -29.0 °C
23.3 ft-lb/in²

@Temperature -20.2 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
Unannealed; ASTM D648
Vicat Softening Point 11.0 °C

@Load 5.10 kg
51.8 °F

@Load 11.2 lb
Rate A (50°C/h); ASTM D1525