Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 41.4 MPa | 6000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87549 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® FRA204 ABS High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Spartech CamAlloy /ABS Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Spartech Korad® SP-9011 Cap ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8006 Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM Data |
Styron Magnum™ 2642 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM Data |
Styron Magnum™ 348 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM Data |
Styron Magnum™ 800 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D 638 |
Styrolution PS 2610 GPPS Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution |
|||
Tensile Strength, Yield | 41.4 - 89.6 MPa | 6000 - 13000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, Annealed Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3300 Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 41.4 - 89.6 MPa | 6000 - 13000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), Annealed Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall UV-6670 Rigid PVC, Molding Georgia Gulf UV-6670 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Bapolan® 6055 Polystyrene, Injection Molding Bapolan PS6055 is a crystal polystyrene resin designed for injection molding applications requiring fast cycle times and superior optical properties. It complies with US FDA21 CFR177.1640 and 94HB .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall 5055 Rigid PVC, Extrusion, White Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall 7555 Rigid PVC, Extrusion, Natural Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall 6509 Rigid PVC, Molding Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall 9202J Rigid PVC, Molding Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive produ.. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D-638 |
Axiall 3027 Rigid PVC, Extrusion Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM 638 |
PlastxWorld CEVIAN® SER20 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |